Asphalt road

surface
Call Us
More than expected

What will you get from
basalt fiber reinforced asphalt concrete?

It is easy to fit adding of basalt fiber into the technological process of an asphalt concrete mixture preparing.

Since the operating temperature range of fiber starts at –260°C and ends at +680°C, this material can be successfully used as a reinforcing additive for asphalt concrete.

Z

High coating strength

Hundreds of millions of reinforcement points in every cubic meter of mix create an effective 3D reinforcement matrix.

Z

Increased durability

Reinforcement with basalt fibers significantly increases the durability of the asphalt concrete pavement.

Z

Rut reduction

Technobasalt® Fiber binds perfectly the particles of asphalt concrete mixture and hardens it at any operating temperature.

Z

Good reputation

High quality road surface is good for further commercial transactions.

Cut of the pit of the asphalt concrete pavement reinforced with Technobasalt® basalt fiber

Has your company applied 
basalt fiber yet?

You can contact us and get a preliminary consultation from our technical specialists. In addition, if you are interested, we will provide your company with the necessary amount of fiber for an independent experiment and tests of our product in the asphalt concrete mixture.

Recommendations for application
of basalt fiber in asphalt concrete pavement

Asphalt hot mixes based on polymer-modified bitumen

Reinforcement recommendations:

Fiber: Technobasalt® Fiber RBR-18-T16/5 (1%)

  • monofilament diameter 18 (16) microns;
  • sizing type T16;
  • fiber length 5 mm;
  • fiber moisture 1%.

Fiber consumption: 3-4 kg/ton of mixture.

Features of the fiber introduction into the mix: uniform dosage.

Asphalt concrete SMA-10, SMA-15, SMA-20

Reinforcement recommendations:

Fiber: Technobasalt® Fiber RBR-18-T16/5 (1%)

  • monofilament diameter 18 (16) microns;
  • sizing type T16;
  • fiber length 5 mm;
  • fiber moisture 1%.

Fiber consumption: 3-4 kg/ton of mixture.

Features of the fiber introduction into the mix: uniform dosage.

Gusasphalt (cast asphalt mix)

Reinforcement recommendations:

Fiber: Technobasalt® Fiber RBR-18-T16/5 (1%)

  • monofilament diameter 18 (16) microns;
  • sizing type T16;
  • fiber length 5 mm;
  • fiber moisture 1%.

Fiber consumption: 1-2 kg/ton of mixture.

Features of the fiber introduction into the mix: uniform dosage.

How others do it

Examples of asphalt pavements reinforced with
Technobasalt® Fiber

Cherkasy Automobile Bridge

This project is interesting from the point of view of performing work at a facility of strategic importance with a fairly high throughput. In the construction of an asphalt concrete roadbed, Technobasalt® Fiber was used.

More details

Assistance with calculations

Through the efforts of the Technobasalt team and together with some design institutes, we have brought together the entire range of data necessary both for understanding the properties of the material and directly for performing design calculations.

You can download this guide using the current link

Basalt Materials Handbook Technobasalt

We have collected the most common asphalt mixes in one brochure. This will help you in your work.

Technical solutions for basalt reinforced asphalt-concrete pavements

Your question

6 + 8 =

Address

01010, Ukraine, Kyiv
Omelyanovycha Pavlenko 4/6
office 14/10
Technobasalt Invest LLC

Phone

+380 44 280 93 61

Mobile phone

+380 67 557 07 61

E-mail

sales@technobasalt.com